How to minimize post welding defects?

user-image
Question added by Bijo David , Production Engineer , NBTC
Date Posted: 2017/01/25
Jeffrey Macasusi
by Jeffrey Macasusi , Welder , GSE$C

Adjust the right electric current and voltage of the welding machine and always clean the metal or plate using buffing disc or grinder disc before start the welding.