What weld defect often occurs weeks after welding the joint?

user-image
تم إضافة السؤال من قبل Ralph Bateman , Sr Welding Engineer , AF Global Corporation
تاريخ النشر: 2013/10/25
muhammad rizwan ullah
من قبل muhammad rizwan ullah , SHALL GTL , DOOSAN BLACKAT

DUE TO PRO CITY OR  LACK OF FUSION  

Ralph Bateman
من قبل Ralph Bateman , Sr Welding Engineer , AF Global Corporation

The defect I was looking for is referenced as HIC (Hydrogen Induced Cracking)... a sneaky lil defect primarily caused by poor heat management, particularly when not managing the cooling rate properly. Results can be catastrophic!

ardel garcia
من قبل ardel garcia , fitter/welder , amadeus marine LTD.

low amperage or no grinding

Anton Bester
من قبل Anton Bester , Mentor Mechanic , Bancroft Global

When you not treed the welding spot with head treetment after it wash weld it will start to cold crac on that spot ofter weeks

Omar Uzcategui
من قبل Omar Uzcategui , Welding and Inspection Team Leader , Petrochemical of Venezuela

Defect often occurs after welding is crack in Carbon Steels Cr-Mo (P3-P4 and P5 Numbers for Asme Code)

ROHITKUMAR RAKHOLIYA ROHIT
من قبل ROHITKUMAR RAKHOLIYA ROHIT , MANAGER , PRODUCTION & PLANING

THE WELD DEFECT OFTENLY OCCURS IS COLD CRACK.

Mohamed Abdel Raheem Abdel Kader
من قبل Mohamed Abdel Raheem Abdel Kader , QC Engineer , Petojet

hydrogen cracks

this problem can solved by using low Hydrogen electrods

Shaheen K M
من قبل Shaheen K M , QHSE Engineer , Shine Star Eng. Steel & Welding LLC

Cold cracks..